Language

Your Searchresult for: Composite parts
General purpose and laminating resins Material attributes Heat resistance (HDT) Pot life 200 g / 20°C
AH 110 / SR

Downloads:
  • medium viscosity
  • fast curing
  • high heat resistance
  • unfilled
  • high strength
94 ± 3 13 - 15
AH 110 / TGL

Downloads:
  • unfilled
  • high strength
  • high heat resistance
  • medium viscosity
101 ± 3 55 - 65
AH 140 / TC 60

Downloads:
  • low viscosity
  • high heat resistance
  • good curing at room temperature
  • excellent wet-out characteristics
  • high strength
97 ± 3 55 - 65
AH 140 / LI 20

Downloads:
  • cures tack free
91 ± 3 18 - 22
AH 140 / TC 90-1

Downloads:
  • unfilled
  • very low viscosity
  • long processing time
  • high heat resistance
  • high strength
  • excellent wet-out characteristics
90 - 105
AH 140 / LI 60

Downloads:
  • cures tack free
  • high heat resistance
105 ± 3 50 - 60
AH 140 / LI 130-2

Downloads:
  • cures tack free
  • high heat resistance
  • long processing time
107 ± 3 120 - 140
LH 25 / Resin+Hardener

Downloads:
  • flammability classification S 4
  • smoke emission class SR-2
  • drippability class ST-2
  • dimensionally accurate
  • test of toxicity of smoke gases - Annex C
90 ± 3 50 - 60
LH 28-1 / TM

Downloads:
  • very high heat resistance, depending on post curing till 175 °C
  • long processing time
  • low exothermic character
  • heat curing
175 ± 3 240 - 360
LH 30 resin+hardener

Downloads:
  • medium viscosity
  • low exothermic character
  • heat curing
  • very high heat resistance
  • long processing time
181 ± 5 160 - 200
BLH Epoxy 200 / K 25

Downloads:
  • low viscosity
  • good curing at room temperature
  • excellent soaking of aramid fibre cloth
  • excellent soaking of glass fibre cloth
  • excellent soaking of carbon fibre cloth
  • certified according to "Germanischer Lloyd"
BIV Epoxy 800/BIV 800

Downloads:
  • very low viscosity
  • long processing time
  • certified according to "Germanischer Lloyd"
85 ± 3 260 - 300